Stanley 929All position DC as well as AC inconel electrode. Extremely easy slag removal.
 |
|
Overview |
|
Specifications |
|
Email to a Friend |
|
A Niobium bearing, all position Inconel electrode for joining high temperature and cryogenic steels and nickels
- Excellent out of position.
- Phenomenal physical properties.
- Extremely easy slag removal.
- Performs unusually well on AC current.
- Also available in TIG form as product code S929 TIG.
|
|
Overview |
|
Specifications |
|
Email to a Friend |
|
APPLICATIONS:
For dissimilar welds on nickel base alloys to themselves, to alloyed steels or to stainless steels.
MICROSTRUCTURE:
In the as welded condition this nickel base weld metal consists of austenite with a few carbides.
FLUX COLOR: Grey
TYPICAL MECHANICAL PROPERTIES:
Undiluted Weld Metal
Tensile strength
Yield strength
Elongation |
Maximum Value Up to:
100,000 PSI (700N/mm2)
60,000 PSI (420N/mm2)
43 %4 |
RECOMMENDED CURRENT: DC Positive (+) or AC
TEMPERATURE RANGES:
| Diameter (mm) |
3/32(2.5) |
1/8(3.25) |
5/32(4.0) |
| Minimum Amperage |
50 |
70 |
90 |
| Maximum Amperage |
70 |
95 |
120 |
WELDING POSITIONS: Flat, Horizontal, Vertical Up, Overhead
RECOMMENDED AMPERAGE SETTINGS:
Diameter
(mm) |
Length
(mm) |
Weldmetal/
Electrode |
Electrodes per lb
(kg) of Weldmetal |
Arc Time of
Deposition
min/lb (kg) |
Amperage
Setting |
Recovery
Rate |
| 3/32 (2.5) |
14" (350) |
.37oz (10.5g) |
43 (95) |
37 (82) |
60 |
105% |
| 1/8 (3.25) |
14" (350) |
.76oz (22g) |
21 (47) |
24 (53) |
90 |
105% |
| 5/32 (4.0) |
14" (350) |
1.14oz (32g) |
14 (31) |
17 (38) |
105 |
105% |
WELDING TECHNIQUES:
Weld at minimum amperage to maintain low heat imput.
ELECTRODE PACKAGING & DIMENSIONS:
| Diameter(mm) |
3/32(2.5) |
1/8 (3.25) |
5/32 (4.0) |
| Length (mm) |
12" (300) |
14" (350) |
14" (350) |
| Electrodes / lb |
24 |
13 |
9 |
| Electrodes / kg |
53 |
28 |
19 |
|
|
Overview |
|
Specifications |
|
Email to a Friend |
|
|
|
|
|
|